The BFS/HL sorbent was prepared at a weight ratio of 30/70 with a slurrying time of 16h and a slurrying temperature of 65℃.
The BFS/HL sorbent was prepared at a weight ratio of 30/70 with a slurrying time of 16h and a slurrying temperature of 65℃.
炉石/氢氧化钙吸收剂重量配比为30/70,于65℃浆化16小时后乾燥后研磨制备而成。